This case demonstrates the debinding stage of SiC ceramic components in our 800°C debinding furnace,showing the critical weight reduction and dimensional stability achieved after binder removal.



latest company case about [#aname#]


Process Overview
1. Pre-Debinding Stage: Hexagonal SiC green bodies, formed by our hydraulic press, were weighed andmeasured to record initial weight and dimensions.


2. Debinding in Action: The parts were loaded into the 800°C debinding furnace for controlled thermaltreatment to remove organic binders.


3. Post-Debinding Verification: After debinding, the components were re-weighed and re-measured,confirming consistent weight reduction (target binder removal rate achieved) with no deformation orcracking.


latest company case about [#aname#]

latest company case about [#aname#]



Key Takeaway
Our debinding process ensures complete binder removal while maintaining precise dimensional accuracy,preparing the parts for the next high-temperature sintering stage in our 2200°C furnace.